Lighting reflector - mirror finish overlay





2004

I'm running a lighting fixture factory and am using aluminium (mirror finished) sheet as the reflector on the recessed lighting fixtures for office and commercial use. Due to price competition becoming harder and harder, I have to look for a cheaper material to replace the existing al. sheet. Had heard from people that there's some kind of overlay with mirror finishing on one side that can stick onto metal surface. By using such kind of overlay, the cost will be more competitive than my existing material. Would be much appreciative if anyone can keep me update / advice on such material. Thank you.

Regards,

David Ng
lighting industry - Hong Kong, Guangdong, China



Its called Vacuum Metallising.

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind
supporting advertiser
Bengaluru, Karnataka, India
saify logo
2004


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"