Removing weather stain from stainless steel





We are importer of stainless steel material. It happens that they are left under rainy condition and they get stain and yellow color. How is it possible to get rid of the stain and the color.

Massoud Sharif
importer - Thornhill, Ontario, CANADA
2004


Why don't you just buff the stains out?

Michael Georgiadis
hobbyist - Durban, South Africa
2004


Buffing may be very time consuming dependent on the amount of material and degree of discolouration. You could try dilute acid to activate the chrome, acid dependent on stainless steel type. Remember to protect yourself and the environment.

Robert Sachs
- Morrisburg, Ontario, CANADA
2004



It is easy to remove these stains with citric acid formulations that are available on the market.

Adv.
Contact us if you need help.

lee kremer
lee kremer sig
Lee Kremer
Stellar Solutions, Inc.
supporting advertiser
McHenry, Illinois
stellar solutions banner
2004



Adv:

Any stains on Stainless steel will quickly be removed using our Scratch-B-Gone kit with very little effort. In fact weld mark and heat scorch also comes out quickly.

Barry Feinman
Barry Feinman - Chief Restoration Officer
BarrysRestoreItAll
supporting advertiser
Carlsbad, California
barrysrestoreitall


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"