Conductivity of zinc-chromate electroplating materials


(1999)

I'm looking for products and electrical conductivity information related to zinc-chromate electroplated materials. Specifically, clear chromate products for cold rolled steel that resist fingprinting and provide high electrical conductivity.

Fred Nance



(1999)

We have been using zinc chromate on CRS for our chassis and we have recently learned about zinc whiskers. I cannot offer any support to your question, however maybe some one will know your answer and be able to suggest an alternative protection to eliminate our zinc whisker problem.

Alan Fitzgerald
- Mesa, Arizona


(2001)

I have read an article concerning zinc whiskers growing on the bottom of access floor panels used in computer room as flooring. Most of these utilize electroplated steel on the bottom. I am trying to find information about procedures for testing the panels to see if they have zinc whiskers and if they do a procedure for cleaning/removing them from the panels.

Paul Henderson
environment services - Londonderry, N.H. USA


Ed. note-- please see our FAQs on zinc and cadmium whiskers



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.