I need information about aluminum die casting specifically for ADC12 (equivalent to ASTM SC102A or SAE303). If possibble, the microstructure, alloy composition etc.

ASRI A.M.

Asri Amat Mokito
- Malaysia


(2005)

ADC12

Component
Cu
Si
Mg
Zn

Wt. %
1.5¡ã3.5
9.6¡ã12.0
0.3¥H¤U
1.0¥H¤U

Component
Fe
Mn
Ni
Sn

Wt. %
1.3¥H¤U
0.5¥H¤U
0.5¥H¤U
0.3¥H¤U


Al : Remainder
Physical Properties
Metric

Density
2.7 g/cc

CTE, linear 20¢XC
21 £gm/m-¢XC

Heat Capacity
0.963 J/g-¢XC

Thermal Conductivity
92 W/m-K

Melting Point
515 - 580 ¢XC

Solidus
515 ¢XC

Liquidus
580 ¢XC


I hope this will be great useful to you

from
gv

Venkatesan.G
- Chennai, Tamilnadu, India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.