Want dark bright nickel finish to be whiter





2003

Our competitor sells bright nickel brightener with a whitish bright finish. Ours is mirror bright but more on the darker bright side.

Could anyone tell me what particular component would give our brightener that whitish finish.

Thanks.

Ma. Karenina Simon
- Mandaluyong, Manila, Philippines


Hi, Simon. I don't recall seeing the answer to your question in print, but perhaps a close study of the literature, including patents and expired patents, would give you some answers.

Things may be different in the Philippines than in the U.S., but here it is considered improper to ask people to reveal the trade secrets of your competitors :-)

Good luck with your research.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2003


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"