Nickel Electroless plating Testing Methods





2003

Dear sir,
We are planning to start a Electroless Plating for Pins. We have already deposited 30 microns of nickel, now we have to do the salt spray testing we want know the methods of this testing and certifying body for these kind of plating in India.

We would also like to ask you is there any study material on this subject.

Regards, Balaji.

R. Balaji
- COIMBATORE, TAMIL NADU, Tamilnadu, India


"Electroless Nickel Plating" book by Wolfgang Riedel is a good buy.

Balaji Mandulapalli
- Miami, Florida
2003


none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages

Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"