-----Plating onto Carbon
I am trying to find information on plating of chromium (also copper and nickel) onto carbon. The carbon is either in the form of a powder, or a film held together by a polymer. Any information or insight on this would be much appreciated.
Rich BraunMaxwell Technologies - San Diego, California
1998
Are you looking for decorative finish or engineering finish? If nothing else works, I would suggest a vacuum metallizing method.
Mandar Sunthankar- Fort Collins, Colorado
1998
--
Mr. Braun:
Our FAQ about plating onto organic materials may get you started.

Ted Mooney, P.E.