In the literature there is mentioned possibility of addition of Naphtalene Trisulphonic Acid for Hardening Nickel Sulphamate bath .

Does someone has expeince with such bath , and what is the optimal concetration for addition of the additive.

yehuda blau
Yehuda Blau
YB Plating Engineering and Quality - Haifa Israel


(1998)

Dear Yehuda:

NTA can be added to sulfamate Ni baths at concentrations up to 7 - 10 g/l. You want to find your preferred concentration based on the desired hardness, stress level etc. The Nickel Development Institute (www.nidi.org)has a useful brochure - Compendium on Nickel Electroforming (or something like that) which they will mail you free of charge. One paper in there by A. Watson deals extensively with sulfamate bath additives, including NTA.

Best of luck from PlaterB

berl stein
berl sig
"PlaterB" Berl Stein
NiCoForm, Inc.
supporting advertiser
Rochester, New York

nicoform



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.