Sodium Chromate Tetrahydrate?


(1998)

Sodium Chromate Tetrahydrate- Na2CrO4:4H2O,

I have heard of this chemical being used as a chromate treatment on steel, followed by a Sodium Hydroxide dip and oven dry. Who can shed some light on this process?

Dave McKay
- Highland Hts, Ohio


(2007)

Dear Sir,

I want steel gray colour coating on seed glass beads using the cool process of lusturing.

Kindly suggest the name of chemical for the purpose.

I will appreciate & awaiting for early response.

Jagdamba Prasad Chaturvedi
- Valsad, Gujarat, India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.