Plating over pot metal




Can anyone tell me how to chrome plate pot metal, plastics and other none conductive materials and also aluminum. If so can you do it in simple terms.

Thank you,

Jim Cantrell
- Nancy, Kentucky, USA
2003



You can't do it simply, Jim. Multilayer plating with a chrome top layer onto any of these substrates is possible in an industrial setting but it is a large undertaking, beyond what a casual hobbyist would do. And if you intended to plate anyone else's parts you would be operating in a highly regulated industry where permits are mandatory and the regulators eagerly throw violators into jail (although I'm not saying a home-based hobbyist is in serious danger of that unless something went horribly wrong).

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2003


A simple no to the complex question you ask. Three very different means to plate the materials you ask. All specialized, all difficult. Sorry

Jon Quirt
American Bright Works - Fridley, Minnesota
2003


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"