ASTM B-201 vs. ASTM B-1117?

adv.   auto technology banner

(1998)

We would be very grateful if someone could explain us something about ASTM B201-80 [link by ed. to spec at TechStreet] norm and its eventual difference from ASTM ASTM B117 [link by ed. to spec at TechStreet] norm. Thank you in advance.

spina
- Italy


Hello, Spina. B117 specifies how to run a neutral salt spray test and is not specific to any particular finish. B201 describes a number of testing methods for chromate coatings on zinc or cadmium, of which salt spray testing is one method.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.