-----Zinc nickel reel to reel plating
I would like to plate zinc/nickel in a alkaline bath (for reduced surface stress and good formability) on wire in a reel to reel system is there a bath with a high enough current density to be effective. Is it possible to plate in a reel to reel system with a alkaline bath? What chemistry will do this?
Harvey Pierman- Bedford Hts., Ohio, USA
2002
Suggest you contact one of ETL's business partners, Shipley (a Rohm & Haas Company). Please contact me for further info.
James L ForandElectroplating Technologies Ltd. - Coplay, Pennsylvania, USA