Aging solution to give carbon steel coated with zinc a gray aged patina




I'm a craftsman and I'm having a hard time finding an aging solution for my creations. I'm wanting to give it a dark gray aged patina. I use a carbon steel coated with Zinc.

Jeffrey Dean
- Lancaster, P.A., U.S.A
2002



2003

Gray for zinc or zinc plated material:

200 gm iron chloride

1 lit water

Cold immersion(20 min.)!

Good luck! Goran Budija
- Zagreb,Croatia


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"