Electropolishing electroless nickel


(1998)

I am trying to locate appropriate processes to electropolish high phosphorus electroless nickel.

James Buhler
- San Jose, California


(1998)

James Buhler:

We have a process for electropolishing nickel, but I think you might be disappointed in the results on electroless nickel. The reason is that the nickel dissolves in the bath, but the phosphorous does not, leaving a smut on the surface.

We would be happy to run a free sample for you, just to be sure.

Regards,

Ed Bayha
Metal Coating Process Corporation - Charlotte, North Carolina



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.