Restoring finish to aluminum trim on Retro table



I have a 1950's retro table with 3.5 inch polished aluminum trim. Wear and tear has left gouges and scratches in it. What is the best method of restoring the finish on the trim?

Doug Giesinger
- Sherwood Park, Alberta, Canada
2002



Marine Aluminum Restorer and Polish
3m_aluminum_restorer
on Amazon
or eBay
(affil link)

Hi, Doug. Aluminum can be restored to brightness by buffing. Unfortunately, removing scratches requires polishing down to their full depth, which may be too deep to be practical. But good luck with it.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"