ORP values for treating waste water


(1998)

Could someone share specific information on using instruments such as orp meter to regulate oxidation of specific metals in waste water. Water contains ferrous salts in the range of 7000 ppm and we need to control additon of oxidizer. Also may encounter other metals.

James Chunn
- Theodore, Alabama


(2000)

I know that Orion Research has several instruments and electrodes that measure ORP/pH/temp. One particular instrument (250A+) can be calibrated to the SHE, with a standard.

Don Campbell
- League City, Texas



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.