What is phosphating? I am completing a wastewater discharge permit for a Jobshop that paints metals and plastics. Prior to painting, the parts are dipped in a cleaning solution to remove oil and grease. This cleaning solution contains phosphates. Is this phosphating, or is phosphating a different coating procedure?

Robert Adams


Dear Bob, phosphating is the process of providing a conversion coating for iron bearing metals and/or etching/activating for non-ferrous metals. When the metal comes in contact with the phosphate solution, a chemical reaction takes place (also called pickling). The phosphate coating is deposited. The topcoat will now have a better substrate profile in which to adhere to. Remember that aluminum does not accept a conversion coat unless phosphate chrome is used. The aluminum will still receive an etch that will accept good adhesion.

bob utech
Bob Utech
Benson, Minnesota

A Guide to High Performance Powder Coating
by Bob Utech
[link is to Amazon]


Dear Sir:

Many heavy duty cleaners contain phosphates as part of their makeup. You need to determine if the job shop is just degreasing the part or actually applying a phosphate coating.

Phosphate cleaners are typically alkaline, phosphate conversion coatings are typically acidic.

Finally, it is possible to apply a phosphate conversion coating (zinc or iron) to aluminum.

Edward Koneczny
- Birmingham, Michigan


please tell me in detail about accelerators used during phosphating as a paint base; also tell me about the post treatments regarding the phosphating process.



I am a chemist from pakistan. I need some know how about metal pre-treatment system. Is there any gentleman who gives me information about alkaline cleaners, pickling solutions, phosphating chemicals. God bless you.

syed Iqbal Saleem
- pakistan


Hello, Mr. Bapat. Hello, Mr. Saleem,

There are entire shelves and even aisles in technical libraries which attempt to answer your questions, so it is hard to recommend just a single book, but Samuel Spring's "Preparation of Metal for Painting" [link is to info about the book at Amazon] is a book that I can recommend.; or try "Phosphating of Metals" [link is to info about the book at Amazon] by Rausch & Rauch. or "Phosphating & Metal Pretreatment" [link is to info about the book at Amazon] by Freeman. Good luck.

Ted Mooney, Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey

September 22, 2011

What is the difference between phosphate cleaner and phosphate conversion?

harish mehra
employee - delhi, India

September 22, 2011

Hi, Harish. Phosphates, such as trisodium phosphate, are sometimes used as detergents to assist cleaning. But phosphate conversion coating, sometimes called phosphatization, is a pretreatment process for metal which improves its corrosion resistance and provides a good base for the adhesion of paints or absorption of oils. If you can provide some context rather than an abstract question, we can probably assist in more detail. Thanks.


Ted Mooney,
Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey

This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices

©1995-2018, Inc., Pine Beach, NJ   -   About   -  Privacy Policy
How Google uses data when you visit this site.