Biomaterials




Is there any book /literature on "electrochemical polishing required for orthopedic implants".

Vrishali Dalvi
- Mumbai



ASTM has/had a spec ASTM F86 on it.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.



Dear Vrishali,

I am unaware of any books that deal with this subject. Do not despair, the readers of this column are a talented lot. I have previous experience with implantable devices and would be willing to help you in any way I can. Looking forward to hearing the specifics of your questions.

John Holroyd
- Elkhorn, Wisconsin


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"