-----Alodine or Alocrom 1200 conductive replacement
I am looking for an alternative for Alodine or Alocrom 1200. In addition to its corrosion and scratch resistance and use as a paint primer, of great importance is low electrical resistivity. Any proven recommendations?
Colin Pugh- Watford, England
These are used for AMSC5541 chromate conversion coating. Start with that spec, and read the QPL (Qualified Products List); there you will have the names of all the products which are accepted as equivalent.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey