I'm having difficulty finding European sources to black nickel plate on stainless steel. Would like some suggestions please.

Janet Toth
aerospace


(1998)

You cannot plate black nickel directly on stainless steel. First you need a strike nickel, then a bright nickel and only on the top of it you can plate black nickel.

sara michaeli
sara michaeli signature 
Sara Michaeli
chemical process supplier
Tel-Aviv, Israel



(1998)

We plate stainless steel sheets in black, but the plating process involves titanium nitride sputtering. Plating can be done on type 304 (18% chrome and 8% nickel) or 316.

Regards,
Mike

Michael Liu Taylor
Michael Liu Taylor
   specialty stainless steel distributor
Dallas, Texas



(1998)

We do plating on stainless steel, no problem, please reply!

Thanks,

Max T. Faeth
- Los Angeles, California, USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.