Properties of and Applications for Zinc Oxide Whiskers



I like to know more about the properties and applications of Zinc Oxide Whisker.

Ken Fund
- Hong Kong



Out of curiosity, I just did a quick web search on keywords zinc oxide whisker. 68 hits came up, many from China, some from finishing.com archives. Plenty of information out there!

Bill Reynolds
Bill Reynolds [deceased]
consultant metallurgist - Ballarat, Victoria, Australia
We sadly relate the news that Bill passed away on Jan. 29, 2010.

 



August 2008

Hi, Ken. Is this a bit of homework for a school science project, or are you a manufacturer with this product available as a by product, or what? It's difficult for us to help you until you provide some context. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"