Electropolishing of Pure Nickel


Q. I have a sample of Nickel 200 that I want to electropolish. What is the best electrolyte, current, voltage, time, etc. to polish a specimen area of 1.0-0.2 cm^2.

Phillip Hayenga
Washington State University - Pullman, Washington, United States


Q. I have sample of nickel 200 that I want to electropolish. What is the best electrolyte, current, voltage, time, etc to polish a specimen area of 0.10"-0.20"

Moore Miao
FOXSEMICON - Kunshan city, Jiangsu province, China

Q. I want to electropolish pure nickel substrate. We have a small electropolishing unit, and I was wondering what would be the proper electrolyte to use and the voltage of the DC current. My sample size ranges from a thickness of 2 mm to 0.1 mm and width of 2 mm.

Tania Rizwan
University of Houston - Houston, Texas

Electroplating Engineering Handbook
by Larry Durney
from Abe Books


December , 2012

A. Hi. If you are unable to find suggestions for electropolishing of pure nickel, I would expect that the electrolytes, current, voltage, time, etc. would be similar to those used for stainless steels. Many different generic and proprietary formulations have been used, and you can get a good tabulation from the Electrolytic Polishing chapter of the Electroplating Engineering Handbook =>

Good luck.


Ted Mooney,
Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey


Q. I'm from Indonesia, a plastic injection mfg. industry.

I have done nickel electroforming process for making a pyramidal reflective plastic mold; but for the further process of ELECTROPOLISHING I could not find the chemical for it.

Can anyone tell me the chemical supplier and the technical assistance for doing the electropolishing?

Best Regards,

Willy Sasmita

January 24, 2011

Q. I am looking for the same question. I have tried many things but none of them have been suitable yet. I will post the answer as soon as I get some success.


Shikhar [last name deleted for privacy by Editor]
- IISc, India


A. Dear Sir:

Please follow the hyperlink below which will connect you to our web site. You will find information there about chemicals, equipment, and process technology for electropolishing almost any metal.

We can furnish a proprietary solution and technical expertise for electropolishing nickel. Please contact us for further details.

Ed Bayha
Metal Coating Process Corporation - Charlotte, North Carolina

This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices

©1995-2018, Inc., Pine Beach, NJ   -   About   -  Privacy Policy
How Google uses data when you visit this site.