Stone Guard / Stone Hard for Copper Substrates


(1998)

Has anyone heard of a coating called "Stone Guard" or "Stone Hard" applied over a copper substrate?

This coating is apparently used on a machine for sealing the plastic bags found in cereal boxes.

Thanks and Regards

Ken Lemke
Ken Lemke
Burlington, Ontario, Canada


(1997)

Stone Hard and Stone Guard are two of several names for floor covering materials made by Stone Hard. They sell mostly epoxies and polyesters. I thing the names are registered.

James Watts
- Navarre, Florida


(1998)

To: Jim Watts

Thank you for the lead regarding Stone Hard.

Would you happen to have a phone number or information that would help me contact the company?

Thank You

Ken Lemke
Ken Lemke
Burlington, Ontario, Canada

(1997)

While it's certainly gratifying to read something positive about Stonhard here, I must admit that the subject application is not up our alley. Stonhard makes and applies seamless polymer flooring products, linings for secondary containment structures, and some specialty industrial coatings, mainly for use on concrete. Our products are principally based on epoxy, urethane, and vinyl esters.

I don't know about "Stone Guard", but this is not one of our brand names. All of our brand names use the "Ston" prefix.

Fred Pfaff
Stonhard, Inc.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.