(1996)

Dear readers,

I am looking for color charts of anodized tantalum: the colors of the oxide films scale vary nicely with applied voltage (and are beautiful!) and I would like to determine the thickness by comparison to color vs. oxide thickness charts (for a lab class). I know these charts exist but haven't been able to find them. If anybody knows where they are, please let me know,

Gerko O [last name deleted for privacy by Editor]
university - Baltimore, Maryland

P.S. Thanks very much for the replies to my previous question; they were very helpful.


November 29, 2008

Hi, Gerko. Sorry that your question is unanswered. But letter 33261 suggests that the colors are similar to titanium, and the author of that claim can probably help you with some details. Good luck with it!

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.