Summary for hypalon rubber rollers Discussion
Hypalon rubber rollers in pickling line are failing on the surface, and the question asks what might be causing it. Onkar Bhandari, a rubber roller manufacturer in Rohini, Delhi, provides no process details beyond that the rollers are used in a steel pickling line and that the failure is intermittent. The response from the site notes that there is not enough information to diagnose the problem and asks for more detail about what “fail sometimes on the surface” means. No specific cause is identified in the thread, and no corrective action is offered beyond requesting a fuller description from someone familiar with the line. The main takeaway is that the issue cannot be reliably traced from the information given, so more operating and failure details are needed before any meaningful troubleshooting can begin.
Q. We are rubber roller manufacturer supplying to steel pickling line. Our hypalon rollers fail sometimes on the surface. What could be the cause?
Onkar Bhandari
rubber roller manufacturer – Rohini, DELHI
August 19, 2017
A. Hi Onkar. Although you’ve given us nothing at all to go on, hopefully someone with experience running a pickling line will offer a couple of common causes. But give us more detail about what you mean by “fail sometimes on the surface”. Thanks.
Regards,

Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com – Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
August 2017