PVDF coating process parameters



A discussion started in 1999 & continuing through 2017

(1999)

Q. Hi ,

We are a jobwork anodising and powder coating company based in south India.We intend starting a PVDF coating facility.Please can you tell us what are the processes involved in this kind of painting.Also we need to know if we can use our chromating bath for pretreatment in this application.Can we use our existing conveyorised oven for this line. At what temperature is this paint cured.

Thanks,

Jothi

P.Jothi Ramalingam
- Chennai,India


(2000)

A. Dear P. Jothi Ramalingam

The same pretreatment processes you use for powder coating will go very well with PVDF coating too. In fact, chromating will give better corrosion resistance and adhesion to the job. It will depend on the end requirements of the painted job.

PVDF has distinct advantage of outdoor performance, as it has C-F bonds. This means, it will be difficult for UV rays to break this bond energy, thus making PVDF one of the best systems for UV resistance performance. And corrosion resistance (neutral salt spray, as per ASTM B117 [link by ed. to spec at TechStreet] ), can easily expect 3000 hours performance from PVDF!

With Best regards,

Dr.K. Murugan
- Mumbai, India



PVDF oven curing temperature

September 18, 2017

Q. At what temperature and number of hours does PVDF have to be Oven Cured?

Hermie Natividad
Wallvision Corporation - Pasig City, Philippines



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.