Gold bombing - recovery process suggestion




2006

We have started bombing of gold pieces recently using NACN & H2O2.

any suggestion regarding recovery of gold from used liquid will be a great help.

thanks,

MR. BIREN KUMAR. DARUJI
JEWELLERY MANUFACTURER - MUMBAI, INDIA



2006

Please see letters #4215 & #27423 for some suggestions.

Good Luck & Best regards,

Jim Sivertsen
Refining & Alloys - Alden, New York, USA




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"