If ı were you ı would try one bar as a trial and error;
ı would skip sealing and hot seal process.If ” water marks” disappeared without sealing/hot sater process you would focus pretreatment process where before anodizing.Frankly,ı suspect either poor etching/neutralization process or too long dwell time after etching during transfer of bar.On the other hand,you would trial one more bar such as without etching process.so you would compare these trial between each other.As ı said ı would look for problem preatreatment process