Michael, the pattern you describe — film on the dry machine, inconsistent or absent on wet runs, on thin sheet — points toward residue held on the surface rather than a change in the steel itself. Dry sanding on thin stock builds both heat and static, and a fine non-woven roller can then smear fine dust and residue across the surface instead of clearing it. Before changing anything else, run a simple diagnostic on a scrap sheet from the same batch: wipe one section with a clean, dry, lint-free cloth and another with a cloth barely dampened with a mild solvent, then compare under raking light. If the film lifts off, you are dealing with surface residue, and the fix belongs in cleaning and dust control rather than in a different abrasive.
If residue is confirmed, work through the variables one at a time so you know which change actually helped. First, clean the roller often during a run; a loaded non-woven roller stops cutting and starts burnishing dust into the surface, which is exactly how a white film forms. Second, reduce feed speed and pressure slightly to cut heat buildup, and keep the sheets from sitting in their own dust between passes. Third, look at static control on the dry line: grounding the worktable and the sheet path, where the machine allows it, and wiping with an anti-static cloth before the final pass are both worth trying, since you cannot add a wet stage. Keep a fresh fine non-woven pass as the very last step, with light pressure, so the final surface is produced by a clean tool rather than one carrying dust from earlier passes.
One caution: do not chase this by going finer and finer on the dry line. Finer grades on a dry, dusty surface often make the film worse, because they generate more fine dust while removing less of it. Solve the residue first, then judge the finish.