"Cerakote"

Cerakote
Starter Kit
cerakote
on Amazon
or eBay
(affil link)
Cerakote is a very thin (0.0005" - 0.001") ceramic-based 2-component coating from NIC Industries that is applied with normal HVLP (high velocity low pressure) paint spray equipment, then baked for curing.