Standards & Guidelines: Electroplated Plastics

by American Society for Electroplated Plastics

ISBN ‍0138423024, 2nd Edition 1979, 184 pages
ISBN ‍0138423105, 4th Edition 1994, 152 pages

ASEP thumb 1  ASEP contents

Cover and table of contents photo is from the 2nd edition, 1979.



A great reference on everything you'd want to know about chrome plated plastics, including such subjects as design of the plastic parts (wall thicknesses, ribs, bosses, draft angles), common substrates and their properties, mold design, design of the plating racks, extensive information about design for selective plating, when to include copper plating in the cycle and when to avoid it, test procedures, and over 100 references.

The 4th edition adds a chapter on automated plating machines not present in the 2nd edition.

Very hard to find! If you see a copy at a reasonable price, snap it up. If you find other sources, please let us know.

These links attempt to go directly to the book in question:



abebooks_avail

"Available" or "Sorry!" note is based on a recent finishing.com search and is not an official position of the bookstore.

Inventory at book dealers varies, and these links might redirect if the volume is out of stock, so please check that the offered book/edition is what we illustrate/discuss here and that you want. If a link doesn't work or points to the wrong book, the dealer may be out of stock; please try another source. Disclosure: finishing.com may receive a commission if you buy after following these links.


©1995-2017 finishing.com, Pine Beach, New Jersey, USA