Need Info About Kanigen Process




2001

Dear Sir.

In our Co.we process PVC film, and we use an element where the film is take out.This rotator has a "Kanigen" application.

Would you please send me more information for this treatment.

Best regards

Ruben Gonzolez, Maintenance Chief
plastics - Pblo.Capitan Artigas,Canelones,Uruguay


Kannigen is the original trade name for electroless nickel when it was fist marketed.You should be able to use medium or high phos. electroless nickel for your application.

Todd Osmolski
- Charlotte, North Carolina, USA
2001


Kanigen is also a Japanese Company name Providing Electroless Nickel Plating Solution and Plating services. If your product or machine is Japanese manufactured likely, it they had done it.

Jim
- S'pore
2001


Ed. note: Thank you, Jim. This is a place of camaraderie and we have dozens of regular readers with your first name, so full name next time please.

Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"