-----Need a mil spec sheet for plating of sheet metal
Hello,
I am a shipping/packing supervisor for a plating company. I also receive the parts when they come into our shop and some of the customers use Milspecs on there Purchase orders. I need to know where I can find a Mil spec sheet for plating of sheet metal. We do zinc, Alodine, anodize and silver. Please help if you can.
- Terrell, Texas USA
2000
Check out the FAQ section; it has some very good links to specification sources.

James Totter, CEF
- Tallahassee, Florida
2000