"What chemicals are used to coat various plastic films that create the iridescent effect"



2000

GREETINGS: What is/are the chemicals that are used to coat various plastic films that create the iridescent effect? Does the film have an effect on the iridescence? If these questions are out of your area of expertise please let me know where I might go for the info. THANKS

William E. Koehler
- North Bergen,NJ USA
^


2001

There is actually a kind of film which is called iridescent film. It consists of multilayer of different plastics and by precisely controlling the thickness of each layer and the kind of plastic. It can create a strong iridescent effect. This must be much simpler instead of applying a coating onto the plastic film.

Patrick Wong
Engelhard Asia Pacific (China) Ltd. - Hong Kong
^

none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages

Q, A, or Comment on THIS thread SEARCH for Threads about ... My Topic Not Found: Start NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact    -    Privacy Policy    -    ©1995-2021 finishing.com, Pine Beach, New Jersey, USA