Please help me. I am doing a project testing different passivation techniques on stainless steels. To begin my experiments I need as many different types of solutions as possible to passivate my SS coupons with.

However the only place which I can find to give me exact solution compositions for free is from Stellar Solutions. All standards on passivation that I can find seem to cost at least $30 - $40. Can anyone recommend a webpage or send me on some data urgently. I plan to use as many variables as possible in my experiments such as different chemicals, different compositions, time and temperature. Any data on the effects of varying these or on any other important variables would be greatly appreciated.

Finbarr Brown
- Dublin, Ireland


(2000)

Most specs from commercial organizations like ANSI, ASTM, ISO are indeed copyrighted. However, United States military specifications are available at no charge, so I'd suggest working with them. See our FAQs on the subject. I don't know where to get stainless steel coupons for free :-)

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.