Epoxy Ink Fisheyeing: Serious Powder Coating Issue

Summary for epoxy ink fisheyeing Discussion

Epoxy ink fisheyeing is the issue raised in this thread: Randy Matuskey of Scottsdale, Arizona asks why a 2-part epoxy ink is fisheyeing when screen printing on TGIC-polyester powder coating. The excerpt provided contains only the question and does not include any replies, so no diagnosis or remedy is stated in the source text. Based on the thread as shown, the key problem is an apparent wetting or surface-contamination issue between the ink and the powder-coated substrate, but the archive excerpt does not supply a confirmed cause. Because there are no answer posts in the provided text, no named expert advice can be attributed and no differing views are present in the excerpt.

Q. Why is my 2 part epoxy ink fish eyeing when screen printing on TGIC-polyester powder coating

Randy Matuskey
– Scottsdale Arizona
September 10, 2024