Summary for electroless nickel plate tubes Discussion
Need EN on O.D. of 10 foot long stainless tubes is a plating RFQ asking for an outfit that can electroless nickel plate SS304 tubes measuring 125 mm ID x 13 mm OD x 3200 mm long, with about 0.015 mm buildup on the outside only. Paul Carter of Waterboro, Maine said he preferred a shop in northern New England, though that was not required. The page excerpt does not include technical replies or shop recommendations, only an editor’s note that the request is outdated but technical responses are still welcome and readers may post their own RFQs. Because no answers are shown, there is no consensus process or conflicting advice to summarize beyond the original job requirements.
RFQ: Looking for A Plating outfit that can Electroless Ni Plate our SS304 tubes that are 125 mm ID x 13 mm OD x 3200 mm long.
Only need about .015 mm Build up on OD only.
Hopefully in northern New England but not mandatory.
Paul Carter
– Waterboro Maine
February 27, 2021
Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).