Overview table of plating and its properties is the kind of reference Fredrik was looking for: a single source covering electroless and electrolytic plating, common metals and alloys, precious metals, and a long list of properties such as composition, internal stress, melting point, density, thermal expansion, resistivity, hardness, wear, corrosion, solderability, and weldability. The reply says this is a tall order and that no one source fully meets it. The closest recommendation given is William Safranek’s *The Properties of Electrodeposited Metals and Alloys*, suggested by name as the best available reference, though it still falls short of the complete table Fredrik wants. The discussion therefore points to a partial but useful handbook rather than a comprehensive all-in-one database.
Q. Does anyone know if there is a book or website covering “all plating” with layer properties?
I know that there is a difference between different processes. Without a more comprehensive one I know that there are lots of good tables over different plating, but if there is something more collected …?
Electroless and electrolytic
both the common metals and alloys as well
precious metal and precious metal processes
preferably in table form
COMPOSITION
STRUCTURE
INTERNAL STRESS
FINAL MELTING POINT
DENSITY
COEFFICIENT OF THERMAL EXPANSION
ELECTRICAL RESISTIVITY
THERMAL CONDUCTIVITY
SPECIFIC HEAT
MAGNETIC COERCIVITY
TENSILE STRENGTH
DUCTILITY
MODULUS OF ELASTICITY
Hardness
Hardness heat
COEFFICIENT OF FRICTION
TABER WEAR
TABER WEAR heat
Corrosion and other properties as Solderability, Weldability, etc.
Fredrik stew
– Gothenborg sweden
February 21, 2021
“The Properties of Electrodeposited Metals and Alloys”
by William Safranek

on Amazon
or
or
(affil link)
A. Hi Fredrik. That’s a tall order, and the closest I know of — although still falling short of what you’d like — is Safranek’s “The Properties of Electrodeposited Metals and Alloys” ⇨
Luck & Regards,

Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com – Pine Beach, New Jersey