Electroless Plating Inside Container: Smart, Useful Search Tips

Summary for electroless plating inside container Discussion

Electroless plating inside a large container is discussed as a practical search-and-research problem rather than a step-by-step process. Pedram VG of Iran asked how to internally electrolessly plate a very large container, about 4 meters long and 3 meters in diameter. The reply notes that the container’s material and exact use were not given, but points out that tanker cars have been electroless nickel plated, suggesting the idea is feasible in similar large vessels. The answerer advises that most available articles are dated and recommends searching under the trade name "Kanigen" instead of only "electroless nickel," because that term may lead to better references. A specific literature search suggestion is given: try "Tanker car Kanigen" on surfacequery.com or scholar.google.com. The thread ends with Pedram thanking the responder, and no alternative methods or conflicting opinions are offered.

Q. WE HAVE A BIG CONTAINER THAT HAS A 4 METER LENGTH AND 3 METER DIAMETER. HOW IT CAN BE ELECTROLESSLY PLATED INTERNALLY? ANY IDEA?

Pedram VG
– IRAN
September 10, 2019

A. Hi Pedram. You have not told us what this container is or its material of construction, but tanker cars have been electroless nickel plated. Most articles about are a bit dated and you’ll probably make better progress using the tradename “Kanigen” rather than ‘electroless nickel’.

Try a literature search of “Tanker car Kanigen” at surfacequery.com or scholar.google.com

Luck and Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.

September 2019

thumbs up sign Many thanks for your answer.

Pedram VG [returning]
– Isfahan, iran
September 11, 2019