Galvalume Coils Have Non-adherent Bleeding Chromate Stains

May 2, 2018

Q. Hi

I have Galvalume coils with an AZ-55 SS 80 CLASS 1, ASTM A924, ASTM A792 (LATEST) ACRYLIC RESIN, NO OIL, REG SPANGLE.

When we de-can the coils, we note fresh water & chromate (yellow) bleeding stains, some of which can be wiped off.

Can you tell me the cause of this condition, i.e., is it a mill defect

Thanks

keith

keith burge
- Pearland, Texas, USA



If you have a question in mind which seems off topic, please Search the Site

ADD a Q, A, or Comment on THIS topic START an UNRELATED topicView CURRENT HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2019 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.