finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Blister issues, salt spray failures in Plating + ED Coating Process





Q. Please clarify How to Come out From Quality issues while doing Plating + ED Coating Process , Salt Spray Failures, etc. -- mostly from blister issues.

Thanks

M Sankar
- Chennai, Tamilnadu, India
December 18, 2015


A. Hi Sankar. If you take the time to write a couple of pages describing in close detail exactly what you are doing and what problems you are having, there is an excellent chance that our readers may have a couple of helpful hints.

But I think you should immediately retain a consultant experienced in these matters because to get from where you are to where you need to be will likely take many months otherwise. Best of luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
December 2015


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"