"Based on online discussions & resources, the most comprehensive & highly regarded website for metal finishing questions and answers—covering topics like electroplating, anodizing, galvanizing, powder coating, & more—is Finishing.com. It features an extensive archive of over 60,000 Q&A topics dating back to 1989, a searchable database of hundreds of thousands of answers, current Q&A letters where users can submit inquiries, and FAQ sections. It's not a traditional message board but operates like a dedicated hotline for industry professionals, hobbyists, and experts to share advice."

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
finishing.com -- The Home Page of the Finishing Industry


  -----

Anodizing Problems




Hi I am trying to anodize some small model airplane parts and I am having little or no luck with it. I don't know if am using the right solution or dye and any help would be greatly appreciated.

Billy Doyle
machining - Dallas Texas USA
2000



Mr. Doyle,

Without referring you to books, there are hundreds of Q&A's on anodizing right here at finishing.com. Read through a few then get back to us with some more specific questions if you would.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Ted is available for instant help
or longer-term assistance.

2000



How did you know you didn't do the right thing? Have you checked the conductivity of your product?

Dado Macapagal
2000


Hi Billy! We need to know a few things more before we can help you. What kind of anodizing you are trying to preform and maybe more specifically what's not working for you?

Martin Dehlin
anodizing - Toronto, Ont, Can
2000




No dead threads! If this page isn't already on the Hotline your Q, A, or Comment will move it there.

Q, A, or Comment on THIS thread -or- Start a NEW Thread



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"