Summary for black rhodium replating Discussion
Black rhodium replating is the issue here: Linda Kimsey says two sterling silver rings with black and white diamonds lost their black rhodium finish on the black diamond settings after sizing and steam cleaning, and the jeweler said he could not repair it. She asked whether she could buy a small amount of black rhodium solution or find someone to replate the rings. The thread excerpt provided does not include any replies, so there is no named expert advice or final solution in the source text. The practical takeaway from the question itself is that the missing black rhodium is a finishing problem, not a stone problem, and the likely remedy would be professional replating by a jeweler or plating service rather than a simple at-home fix. Because no answers are shown, the discussion cannot confirm where to buy the solution or who can safely replate the rings.
March 16, 2015
Q. I have two sterling silver rings with black and white diamonds. Both had to be sized, and when my jeweler did this, someone must have steam cleaned the rings and the black rhodium is gone from the black diamond settings… The jeweler says he can’t fix this. They don’t match the other jewelry I have as the settings are very visible.
A clerk at Sears told me she had just read about the black rhodium.. Is there somewhere that I can buy a small amount of black rhodium liquid [adv: black rhodium plating solution on
or
Amazon [affil link]
? Somewhere where I can take or send these two rings to have them replated?? I would really appreciate any help you can give me. Thank you for any suggestion you can give me.
Linda Kimsey
private party – Streamwood, Illinois