CRCA Sheet Hot Dip Galvanizing: Tough 100µm Reality

Summary for crca sheet hot dip galvanizing Discussion

CRCA sheet for hot dip galvanizing is questioned here because the manufacturer, Pratap VK, says their experience shows HR sheet is better suited for hot dip finishes on cable management products. They are being asked by consultants to use CRCA sheet with a 100 micron galvanized coating and want guidance on whether that is practical. The only answer in the thread, from an unnamed respondent, does not directly compare CRCA and HR performance; instead, it cautions that achieving 100 µm on sheet may be difficult and notes that thinner coatings are more easily achieved. So the discussion suggests the main challenge is coating thickness rather than a clear endorsement of CRCA for this application.

November 10, 2014

Q. We supply cable management products in Hot dip galvanised finish, powder coated etc. For Hot dip finish we normally use HR sheets which we find are the best suited for this finish. Some specs are being sent to us asking for CRCA sheet with Hot dip galvanising of 100 microns. Our experience has shown HR to be the best, but is CRCA also suitable?
Request your suggestion to help us talk with the consultants.

Pratap VK
manufacturer – Chennai, Tamilnadu, India

A. You might find difficulty in getting 100µ on sheet. Thinner coatings more easily achieved.

geoff_crowley
Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK


crithwood logo

November 14, 2014