Summary for chrome linings for shotblast machinery Discussion
Chrome or mag linings for shotblast machinery is a short exchange about what "hi Cr" and "hi Mag" linings might mean for shotblast equipment. Muhammad Akram of Akram Engineering Works in Lahore asked for help with high-chrome and high-magnesium linings for machinery he manufactures. In reply, A. F. Kenton said he did not know enough about shot blast machine construction to give specific guidance, but noted that hard chrome plating is a very smooth, low-friction, abrasion-resistant coating often used on machine parts. He suggested searching for a hard chrome plating shop in Pakistan or India for practical help. Kenton also said he did not understand what magnesium had to do with the subject, and wondered whether "mag" might be an abbreviation for magnetic. The thread does not provide a definitive technical answer, only a pointer toward hard chrome plating suppliers and clarification of the terminology.
Q. Dear sir,
We are manufacturing shotblast machinery. Can you help me regarding hi Cr lining and hi Mag lining? Please help me. Thanks, m akram
muhammad akram
engineering works – lahore panjab Pakistan
A. Hi. Unfortunately, I don’t know enough about the construction of shot blast machinery to be able to help you much. Hard chrome plating is a very smooth, low friction, and abrasion resistant coating which is often applied to machine parts. If you search for a hard chrome plating shop in Pakistan or India, they can probably help you.
Sorry, but I don’t understand what magnesium has to do with the subject at all — or is “mag” an abbreviation for magnetic? :-(
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com – Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
October 2014
A. Most abrasive blast system use polyurethane as a liner in their machines of a hard or high durometer. There are no chemical liner treatments that can hold up to the energy forces without breaking down as a flexible coating.

AF Kenton
retired business owner – Hatboro, Pennsylvania
October 13, 2014