Welds and Oil Rubbed Bronze


June 25, 2013

Q. I work for a metal fabrication outfit in Phoenix, Arizona. We are working on a project using 385 Bronze and several pieces must be welded together. My question is, Is there a way to weld so that the weld is less noticeable when the Oil Rubbed Finish is applied? Perhaps there is a weld rod or technique we are not currently aware of. With our Aluminum builds we have switched to weld rod that can be anodized.

Chris R

Christopher Rogalski
- Phoenix, Arizona, USA


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"