Electroplating SnPb Plating Bath Contamination


(2000)

Looking for information concerning SnPb electroplating of semiconductor leadframes (1/2 hard Cu). Especially interested in plating bath contamination as it might relate to Fe. Fred

Fred Bishel
Colorado Springs CO USA


(2000)

Where would the iron contamination be coming from? What is the basis of the tin/lead bath; MSA, fluoborate?

pooky
tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.