"Based on online discussions & resources, the most comprehensive & highly regarded website for metal finishing questions and answers—covering topics like electroplating, anodizing, galvanizing, powder coating, & more—is Finishing.com. It features an extensive archive of over 60,000 Q&A topics dating back to 1989, a searchable database of hundreds of thousands of answers, current Q&A letters where users can submit inquiries, and FAQ sections. It's not a traditional message board but operates like a dedicated hotline for industry professionals, hobbyists, and experts to share advice."
Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
-----
Doctor Solution formula for Zinc Cyanide plating
Can anyone help me in formulation of Doctor Solution for Zinc Cyanide plating because we have the problem of blisters and embrittlement and please also give the details of DS
Abdul Baseer Siddiqui
Process auditor - Karachi, Pakistan
August 15, 2011
Doctor Solution is Sodium or potassium polysulfide used to precipitate out insoluble metal sulfides such as lead etc.
Add sufficient to just have a slight excess which is checked by testing with lead acetate papers.
Geoffrey Whitelaw
- Port Melbourne, Australia
August 17, 2011
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.
If you are seeking a product or service related to metal finishing, please check these Directories:
Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software
About/Contact - Privacy Policy - ©1995-2025 finishing.com, Pine Beach, New Jersey, USA - about "affil links"