Liquid Nitriding EN 19 to a depth of 0.3 mm




one of my jobs has a requirement of nitriding depth 0.1-0.3 mm and its material is EN 19 or En 18.
So I want to know is it possible to achieve this depth in liquid nitriding on above material.

please reply I am waiting for answer.

thanks.

regards

Haridas Dadas
Development - Pune, Maharashtra, India
June 9, 2011



Dear Haridas Dadas,
for the material EN 19, Acheving the depth of 0.1mm (minimum) is possible in liquid/salt bath nitriding.

Kannan Boopahti
- Salem, Tamilnadu, India
July 11, 2011


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"