What anode basket ⇦ huh? material for Cadmium Fluoborate solution?




In cyanide cadmium plating, ball anodes are used in spiral steel holders.
What material is used to hold the cadmium balls in fluoborate cadmium plating solutions?

Harout Marachlian
Consultant - Glendale, California, USA
May 6, 2011



June 15, 2011

Hi Harout,

Both titanium and zirconium anode basket are suitable for cadmium fluoborate plating solution.

Regards,
David

David Shiu
David Shiu
- Singapore



June 16, 2011

I'm afraid that titanium will dissolve quite rapidly in a fluoborate solution. I'm not sure about zirconium, however.

Lyle Kirman

Lyle Kirman
consultant - Cleveland Heights, Ohio


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"